MHR0312SA type
High voltage reisistor
7. ELECTRICAL CHARACTERISTICS
7.1 Temperature coefficient of Resistance
Resistance value will be measured after stabilization at each sequence temperature
for 30 minutes shown in table below. The measurement will be performed at the step 1
to 6 continuously.
The temperature coefficient of resistance will be calculated from the following formula.
The step 2 and 3 will be based on the step 1, and the step 5 and 6 will be based on
the step 4.
The change of resistance value at each temperature will be satisfied Table 1.
Step
Temp.()
1
25±2
2
-15±2
3
-25±2
4
25±2
5
60±2
6
100±2
TCR(ppm/°C) =
R - R0
R0
×
1
t - t0
× 106
R =Actual measured resistance value () at t°C.
R0=Actual measured resistance value () at t0°C.
t =Actual measured value of test temperature.(°C)
t0=Actual measured value of standard temperature.(°C)
7.2 Voltage characteristics
In standard temperature silicone oil ( or same quality liquid ), resistance value will be
measured at 1/10 of the rated voltage, and then at the rated voltage.
However the time of voltage application will be 3 seconds less.
And the voltage will not be applied more than once every 10 seconds.
R variation will be calculated according to the following formula.
The variation will be satisfied Table 1.
R = (Rs-Ro)/Ro×100
Rs = Resistance measured at 1/10 rated voltage.
Ro = Resistance measured at rated voltage.